technical requirement
●Coaxiality and cylindricity (jump measurement) ≤ 0.05mm
●Dynamic balance g2.5
●Straightness ≤ 0.05mm
●Tightness test: air pressure test 6kg, pressure holding for 3 hours, no leakage
●Thickness of chromium plating layer ≥ 120um
●Shaft head conditioning hrc27-30
●Hardness of chromium plating layer HRC ≥ 62
●Surface roughness ras0.02um
●The internal flow passage adopts cross convection structure
●Provide thermal imaging report when the surface temperature difference is within ± 0.5